Mallard Creek Polymers ROVENE® 4106 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 4106 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 4106 is a carboxylated styrene-butadiene emulsion that has a very stiff or "boardy" hand. This binder is recommended as a modifier for other SBR non-woven binders to increase strength and/or reduce tack. ROVENE® 4106 is also low-foaming and hydrophobic.APPLICATIONS: ROVENE® 4106 is recommended for applications in specialty paper, automotive high-strength nonwovens, and filters.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 49 - 51 %
49 - 51 %
Particle Size 0.17 µm
0.17 µm
pH 8.5 - 9.0
8.5 - 9.0
Brookfield Viscosity 75 - 600 cP
75 - 600 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 69.0 °C
156 °F
Chemical Properties Metric English Comments
Styrene Content 90 %
90 %
Descriptive Properties Value Comments
Emulsifiers Anionic