Magyar Aluminum ALO-P90-02 Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALO-P90-02 Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alumina for Polishing
Physical Properties Metric English Comments
Bulk Density 0.300 - 0.500 g/cc
0.0108 - 0.0181 lb/in³
Oil Absorption 32 - 42 %
32 - 42 %
ml/100g
Particle Size 2.0 - 5.0 µm
2.0 - 5.0 µm
d50
20 µm
20 µm
5% max, wet sieve
Specific Surface Area 6.0 - 15 m²/g
6.0 - 15 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 >= 99 %
>= 99 %
Fe2O3 <= 0.040 %
<= 0.040 %
Na2O <= 0.30 %
<= 0.30 %
SiO2 <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
Calcination Degree Low