Magyar Aluminum ALO-Ex30 Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALO-Ex30 Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calcined Alumina. Min 20% alpha-Al2O3.
Physical Properties Metric English Comments
Particle Size 45 - 85 µm
45 - 85 µm
d50
Component Elements Properties Metric English Comments
Al2O3 >= 98.6 %
>= 98.6 %
Determined by difference
Fe2O3 <= 0.050 %
<= 0.050 %
Loss on Ignition(%) <= 1.0 %
<= 1.0 %
Na2O <= 0.50 %
<= 0.50 %
SiO2 <= 0.030 %
<= 0.030 %