MV Labs YB100 Yb(C2H3O2)3·4H2O Ytterbium acetate tetrahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs YB100 Yb(C2H3O2)3·4H2O Ytterbium acetate tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 422.24 g/mol
422.24 g/mol
Descriptive Properties Value Comments
Assay 41% Yb
CAS Number 15280-58-7
Form White powder
Purity 99.999%
Typical Impurities Check with Manufacturer