MV Labs W860 K2WO4 Potassium tungstate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs W860 K2WO4 Potassium tungstate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 326.05 g/mol
326.05 g/mol
Descriptive Properties Value Comments
Assay 56% W
CAS Number 7790-60-5
Form White crystals
Purity 99.99%
Typical Impurities Na<20; Zn<5; Mo, Si<2; Al, Fe, Mg, Mn, Ni < 1 ppm