Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 183.91 g/mol
183.91 g/mol
Descriptive Properties Value Comments
Assay 28% V
CAS Number 13721-39-6
Form White to pale green powder
Purity 99.999%
Typical Impurities K < 100; Al, Si = 10; Ca, Fe = 2; Ba, Mg < 1