MV Labs TE450 (NH4)2TeCl6 Ammonium hexachlorotellurate(IV)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs TE450 (NH4)2TeCl6 Ammonium hexachlorotellurate(IV).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 412.3 g/mol
412.3 g/mol
Descriptive Properties Value Comments
Assay 31% Te
Form Yellow crystals
Purity 99.99%
Typical Impurities Check with Manufacturer