MV Labs TB800 Tb4O7 Terbium(III,IV) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs TB800 Tb4O7 Terbium(III,IV) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 747.69 g/mol
747.69 g/mol
Descriptive Properties Value Comments
Assay 85% Tb
CAS Number 12037-01-3
Form Brown powder
Purity 99.99+%
Typical Impurities Ca, Si = 10; Cu, Fe = 2; Rare Earths < 10 ND