MV Labs TA560 K2TaF7 Potassium heptafluorotantalate(V)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs TA560 K2TaF7 Potassium heptafluorotantalate(V).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 392.14 g/mol
392.14 g/mol
Descriptive Properties Value Comments
Assay 46% Ta
CAS Number 16924-00-8
Form White crystals
Purity 99.99+%
Typical Impurities Si < 30; Mg, Nb < 10 ppm