MV Labs SM400 SmCl3·6H2O Samarium chloride hexahydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SM400 SmCl3·6H2O Samarium chloride hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 364.8 g/mol
364.8 g/mol
Descriptive Properties Value Comments
Assay 41% Sm
CAS Number 13465-55-9
Form Yellow crystals
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Ca = 8; Fe, Mg < 1 ppm