MV Labs RU450 (NH4)2RuCl6 Ammonium hexachlororuthenate(IV)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RU450 (NH4)2RuCl6 Ammonium hexachlororuthenate(IV).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 349.87 g/mol
349.87 g/mol
Descriptive Properties Value Comments
Assay 31% Ru
CAS Number 18746-63-9
Form Black powder
Purity 99.99%
Typical Impurities Ca, Na < 30; Mg <10; Pd, Si < 3 ppm