MV Labs RH485 [Rh(NH3)5Cl]Cl2 Chloropentaminerhodium(III) chloride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RH485 [Rh(NH3)5Cl]Cl2 Chloropentaminerhodium(III) chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 294.42 g/mol
294.42 g/mol
Descriptive Properties Value Comments
Assay 35% Rh
CAS Number 13820-95-6
Form Pale yellow powder
Purity 99.99%
Typical Impurities Si < 20; Ir, Pt < 10 ppm