MV Labs RB490 RbClO4 Rubidium perchlorate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RB490 RbClO4 Rubidium perchlorate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 184.94 g/mol
184.94 g/mol
Descriptive Properties Value Comments
Assay 46% Rb
CAS Number 13510-42-4
Form White powder
Purity 99.99%
Typical Impurities Cs, K < 50; Al = 10 ppm