MV Labs PT410 PtCl4 Platinum(IV) chloride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PT410 PtCl4 Platinum(IV) chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 366.9 g/mol
366.9 g/mol
Descriptive Properties Value Comments
Assay 58% Pt
CAS Number 13454-96-1
Form Brown crystals
Purity 99.99%
Typical Impurities Si < 10; Na = 2; Ag, Al, Ca, Cr, Fe < 1 ppm