MV Labs PR700 Pr(NO3)3·6H2O Praseodymium nitrate hexahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PR700 Pr(NO3)3·6H2O Praseodymium nitrate hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 435.02 g/mol
435.02 g/mol
Descriptive Properties Value Comments
Assay 32% Pr
CAS Number 15878-77-0
Form Green crystals
Purity 99.999%
Typical Impurities Ca < 4; Si < 2 ppm; Rare Earths < 10 ND