MV Labs PD400 PdCl2 Palladium(II) chloride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PD400 PdCl2 Palladium(II) chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 177.31 g/mol
177.31 g/mol
Descriptive Properties Value Comments
Assay 60% Pd
CAS Number 7647-10-1
Form Brown powder
Purity 99.999%
Typical Impurities Ca = 2; Cu, Zn, Ag, Fe, Mg, Na, Pt < 1 ppm