Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 245.19 g/mol
245.19 g/mol
Descriptive Properties Value Comments
Assay 85% Pb
CAS Number 7783-46-2
Form White powder
Purity 99.995%
Typical Impurities Si < 20; Ag, Ca < 5; Fe, Mg, < 1 ppm