MV Labs PB200 PbBr2 Lead(II) bromide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PB200 PbBr2 Lead(II) bromide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 367.01 g/mol
367.01 g/mol
Descriptive Properties Value Comments
Assay 56% Pb
CAS Number 10031-22-8
Form White powder
Purity 99.999%
Typical Impurities Ag, Ca < 3; Fe, Mg, Si < 1 ppm