Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 303.25 g/mol
303.25 g/mol
Descriptive Properties Value Comments
Assay 68% Pb
CAS Number 7446-14-2
Form White powder
Purity 99.999%
Typical Impurities Ag, Ca < 4; Fe, Mg, Si < 1 ppm