MV Labs NH900 (NH4)H2PO4 Ammonium dihydrogen phosphate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NH900 (NH4)H2PO4 Ammonium dihydrogen phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 115.03 g/mol
115.03 g/mol
Descriptive Properties Value Comments
Assay 27% P
CAS Number 7722-76-1
Form white crystals
Purity 99.999%
Typical Impurities Na, Ca = 5; Fe = 2; Zn, Pb < 1 ppm