Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 144.94 g/mol
144.94 g/mol
Descriptive Properties Value Comments
Assay 88% I
CAS Number 12027-06-4
Form White powder
Purity 99.999%
Typical Impurities Ca, Na = 5; Mg = 2 ppm