Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 53.49 g/mol
53.49 g/mol
Descriptive Properties Value Comments
Assay 66% Cl
CAS Number 12125-02-9
Form white crystals
Purity 99.999%
Typical Impurities Na, K < 5; Fe < 1 ppm