MV Labs ND700 Nd(NO3)3·6H2O Neodymium nitrate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs ND700 Nd(NO3)3·6H2O Neodymium nitrate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 330.25 g/mol
330.25 g/mol
Descriptive Properties Value Comments
Assay 31% Nd
CAS Number 13746-96-8
Form Blue crystals
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Si < 4 ppm; Ca = 5 ND