MV Labs NB550 NH4NbF6 Ammonium hexafluoroniobate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NB550 NH4NbF6 Ammonium hexafluoroniobate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 224.91 g/mol
224.91 g/mol
Descriptive Properties Value Comments
Assay 40% Nb
CAS Number 12062-13-4
Form White crystals
Purity 99.99+%
Typical Impurities Ta = 6; Si < 3; Ca = 2, Al < 1 ppm