MV Labs NA950 NaH2PO4 Sodium dihydrogen phosphate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NA950 NaH2PO4 Sodium dihydrogen phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 119.98 g/mol
119.98 g/mol
Descriptive Properties Value Comments
Assay 19% Na
CAS Number 7558-80-7
Form White lumps
Purity 99.999%
Typical Impurities K < 10; Fe, Pb < 5 ppm