Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs MN100 Mn(C2H3O2)2·4H2O Manganese(II) acetate tetrahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs MN100 Mn(C2H3O2)2·4H2O Manganese(II) acetate tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 245.08 g/mol
245.08 g/mol
Descriptive Properties Value Comments
Assay 23% Mn
CAS Number 6156-78-1
Form Pink crystals
Purity 99.999%
Typical Impurities Cr, Fe = 3; Ca, Mg, Zn < 1 ppm
Users viewing this material also viewed the following: