MV Labs K150 KNaC4H4O6.xH2O Potassium sodium tartrate tetrahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs K150 KNaC4H4O6.xH2O Potassium sodium tartrate tetrahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 282.23 g/mol
282.23 g/mol
Descriptive Properties Value Comments
Assay 14% K
CAS Number 6381-59-5
Form White powder
Purity 99.99%
Typical Impurities Ca <1 ppm