Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 379.38 g/mol
379.38 g/mol
Descriptive Properties Value Comments
Assay 43% Ho
CAS Number 14914-84-2
Form Yellow crystals
Purity 99.999%
Typical Impurities Ca, Si = 2; Ce, Dy, Er < 1 ppm; other rare earths < 10 ND