MV Labs GD870 Gd2(C2O4)3·xH2O Gadolinium oxalate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs GD870 Gd2(C2O4)3·xH2O Gadolinium oxalate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 578.55 g/mol
578.55 g/mol
Descriptive Properties Value Comments
Assay 46% Gd
CAS Number 22992-15-0
Form White powder
Purity 99.999%
Typical Impurities Check with Manufacturer