Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 255.73 g/mol
255.73 g/mol
Descriptive Properties Value Comments
Assay 19% Ga
CAS Number 69365-72-6
Form White crystals
Purity 99.999+%
Typical Impurities Cd, Cr, Cu, In, Si, Zn < 1 ppm