MV Labs FE870 (NH4)3Fe(C2O4)3·3H2O Ammonium iron(III) oxalate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs FE870 (NH4)3Fe(C2O4)3·3H2O Ammonium iron(III) oxalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 428.07 g/mol
428.07 g/mol
Descriptive Properties Value Comments
Assay 14% Fe
CAS Number 13268-42-3
Form Green-yellow powder
Purity 99.999%
Typical Impurities Mn, Ca, Cu, Co < 2; Mg, Ni, Zn < 1 ppm