MV Labs FE700 Fe(NO3)3·9H2O Iron(III) nitrate nonahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs FE700 Fe(NO3)3·9H2O Iron(III) nitrate nonahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 404 g/mol
404 g/mol
Descriptive Properties Value Comments
Assay 14% Fe
CAS Number 7782-61-8
Form Violet crystals
Purity 99.9995%
Typical Impurities Al, Cu = 2; Cr, Co, Mg, Mn, Zn < 1 ppm