Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 482.19 g/mol
482.19 g/mol
Descriptive Properties Value Comments
Assay 12% Fe
CAS Number 7783-83-7
Form Violet crystals
Purity 99.999%
Typical Impurities Mn, Ca, Cu, Co < 2; Mg, Ni, Zn < 1 ppm