MV Labs CU600 Cu2I2 Copper(I) iodide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CU600 Cu2I2 Copper(I) iodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 380.9 g/mol
380.9 g/mol
Descriptive Properties Value Comments
Assay 33% Cu
CAS Number 7681-65-4
Form Light brown powder
Purity 99.999%
Typical Impurities Ag, Ca, Fe = 2; Mg, Si, Zn < 1 ppm