MV Labs CS500 CsF Cesium fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CS500 CsF Cesium fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 151.9 g/mol
151.9 g/mol
Descriptive Properties Value Comments
Assay 87% Cs
CAS Number 13400-13-0
Form White chunky powder
Purity 99.99%
Typical Impurities K, Na, Rb Si < 10 ppm