Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs CS400 CsCl Cesium chloride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CS400 CsCl Cesium chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 168.36 g/mol
168.36 g/mol
Descriptive Properties Value Comments
Assay 81% Cs
CAS Number 7647-17-8
Form White powder
Purity 99.999%
Typical Impurities Rb = 5; K, Na = 1 ppm