Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 168.99 g/mol
168.99 g/mol
Descriptive Properties Value Comments
Assay 35% Co
CAS Number 13817-37-3
Form Red crystals
Purity 99.99%
Typical Impurities Check with Manufacturer