Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 548.23 g/mol
548.23 g/mol
Descriptive Properties Value Comments
Assay 25% Ce
CAS Number 16774-21-3
Form orange crystals
Purity 99.99+%
Typical Impurities Ca, Mg, Fe < 3 ppm