MV Labs BI450 BiOCl Bismuth oxychloride

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs BI450 BiOCl Bismuth oxychloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 260.43 g/mol
260.43 g/mol
Descriptive Properties Value Comments
Assay 80% Bi
CAS Number 7787-59-9
Form White powder
Purity 99.999%
Typical Impurities Cu, Ni, Pb = 1 ppm