MV Labs BE1005 Be4O(C2H3O2)6 Beryllium acetate basic

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs BE1005 Be4O(C2H3O2)6 Beryllium acetate basic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 406.16 g/mol
406.16 g/mol
Descriptive Properties Value Comments
Assay 9% Be
CAS Number 19049-40-2
Form White powder
Purity 99.999%
Typical Impurities Fe, Si = 3; Cu < 2; Al < 1 ppm