MV Labs BA500 BaF2 Barium fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs BA500 BaF2 Barium fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 175.34 g/mol
175.34 g/mol
Descriptive Properties Value Comments
Assay 78% Ba
CAS Number 7787-32-8
Form White powder
Purity 99.995%
Typical Impurities Si < 30; Ca, Sr < 1 ppm