MV Labs AU880 Au(OH)3 Gold(III) hydroxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AU880 Au(OH)3 Gold(III) hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 247.99 g/mol
247.99 g/mol
Descriptive Properties Value Comments
Assay 79% Au
CAS Number 1303-52-2
Form Brown powder
Purity 99.99%
Typical Impurities Na < 100; Ag < 3; Al, Cu, Ni, Pd < 1 ppm