Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 288.33 g/mol
288.33 g/mol
Descriptive Properties Value Comments
Assay 68% Au
CAS Number 13967-50-5
Form White crystals
Purity 99.99%
Typical Impurities Na < 50; Ag < 5; Cu, Ni, Pd, Sn < 3 ppm