Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 197.84 g/mol
197.84 g/mol
Descriptive Properties Value Comments
Assay 75% As
CAS Number 1327-53-3
Form White powder
Purity 99.999%
Typical Impurities Sb £ 5; Fe, Mn < 2; Na £ 1 ppm