MV Labs AL400 AlCl3.6H2O Aluminum chloride hexahydrate

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AL400 AlCl3.6H2O Aluminum chloride hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 241.43 g/mol
241.43 g/mol
Descriptive Properties Value Comments
Assay 11% Al
CAS Number 7784-13-6
Form white crystals
Purity 99.999%
Typical Impurities Cd, Cr, Co, Cu, Fe, Mg, Si, Zn < 1 ppm