Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers NAXELLâ„¢ PC210HR General Purpose Polycarbonate, High MFR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer MRC Polymers
Trade Name NAXELL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers NAXELLâ„¢ PC210HR General Purpose Polycarbonate, High MFR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• Black onlyInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Melt Flow 25 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D 638
Elongation at Break 50 %
50 %
ASTM D 638
Flexural Strength 93.0 MPa
13500 psi
ASTM D 790
Flexural Modulus 2.274 GPa
329.8 ksi
ASTM D 790
Izod Impact, Notched 5.88 J/cm
11.0 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D 648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved