MRC Polymers NAXELLâ„¢ PC117MH General Purpose Polycarbonate, Medium High MFR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer MRC Polymers
Trade Name NAXELL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers NAXELLâ„¢ PC117MH General Purpose Polycarbonate, Medium High MFR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D 792
Water Absorption 0.15 %
0.15 %
ASTM D 570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Melt Flow 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D 638
Elongation at Break 60 %
60 %
ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 2.343 GPa
339.8 ksi
ASTM D 790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ASTM D 648