M. Holland Company SA311 Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company SA311 Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.2 MPa
10900 psi
ASTM D638
Flexural Modulus 3.90 GPa
566 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 0.60 %
0.60 %
ASTM D1003
Transmission, Visible 89.5 %
89.5 %
ASTM D1003
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding