M. Holland Company PP200 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PP200 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
23/23°C; ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding