M. Holland Company LL508 LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LL508 LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 3.1bProcessing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D638
Elongation at Break 630 %
630 %
ASTM D638
Tensile Modulus 0.145 GPa
21.0 ksi
2% Secant; ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790
Descriptive Properties Value Comments
Form Pellets